PLA settings vary by brand, formulation, printer, nozzle, and cooling. Use the spool label or manufacturer data sheet as the starting point.
| Overture Basic PLA | |
|---|---|
| Setting | Tested value |
| Nozzle temperature | 215c |
| Bed temperature | 65c |
| Cooling | After 3rd Layer |
| Print speed | |
| Retraction | |
| Drying temperature / time | 6 Hour / 55c |
Record brand, product line, color, nozzle, and slicer profile. Re-test after changing nozzle material or diameter.
02/03/2026
I have always wondered why when I print in White, there are always little gaps near edges. At first I just thought that it happens with Black Filament too. I tested it and no it does not print exactly the same. I run Overture Filament only. Years ago I decided to stick with one type of Filament for PLA, PETG, a TPU. I run Calibration for each type material. From what I understand the additives in White that contains Titanium Dioxide. This makes it flow differently and may need to run a slightly higher Temperature.
| PLA Variant | Strength / Toughness | Finish | Print Temp | Best Use Cases | Trade-offs |
|---|
| Standard PLA | Rigid, brittle on impact | Semi-gloss | 190–220°C | General prototypes, indoor organizers | Low heat resistance (~55°C) |
| PLA+ / Tough PLA | High impact resistance | Semi-gloss | 205–230°C | Functional mounts, Packout bins, tools | Slightly higher stringing risk |
| High-Speed PLA | Moderate to High | Semi-gloss | 210–240°C | Bambu Lab / CoreXY high-speed printing | Needs strong part cooling |
| Matte PLA | Moderate (lower Z-strength) | Flat / Non-gloss | 190–220°C | Display models, hiding layer lines | Slightly abrasive; weaker layer bond |
| Silk PLA | Low (splits easily) | Metallic sheen | 205–230°C | Vases, decorative props | Swells after extrusion; slow outer walls |
| PLA-CF (Carbon Fiber) | Very stiff, low flex | Textured matte | 210–240°C | Rigid jigs, frames, cosmetic parts | Requires hardened steel nozzle |
* Functional / Snap-Fit Parts: Use PLA+ or Tough PLA with 3+ walls. * Hiding Layer Lines: Use Matte PLA or PLA-CF. * High-Speed Slicing: Check Max Volumetric Speed (`20+ mm³/s` for High-Speed PLA vs. `12–15 mm³/s` for standard/silk). * Heat Exposure (>55°C / Hot Car): Do not use PLA; switch to PETG or ASA.
* Plastic Spools (Bambu, Sunlu, Polymaker Panchroma): Roll cleanly in the AMS without modification. * Cardboard Spools (eSUN, Overture, PolyTerra): Print reusable plastic rim rings or wrap edges in electrical tape to prevent cardboard dust and retraction jams in the AMS.